After the completion and acceptance of many projects, and even after a period of delivery and use, the most common visual problem of aluminum curtain walls is that the surface is uneven, with waves and bulges appearing under natural light, local depressions, and obvious differences in joint height.
Many people simply attribute it to the skill of installation workers. In fact, the unevenness of aluminum plates is a quality defect caused by the superposition of multiple aspects such as deepening design, keel system, factory processing, on-site installation, and material stress. Especially for aluminum plates, they have a large amount of thermal expansion and contraction, and small deformations can be magnified by light and shadow under sunlight, seriously affecting the overall effect of the facade.
Today, from the two core dimensions of keel layout requirements and aluminum plate factory processing requirements, we will discuss how to control the flatness of aluminum plates from the source and avoid surface roughness defects.
A、Keel system: The "foundation" of the curtain wall. If the keel is uneven, the board must be uneven
The keel is the supporting skeleton of the aluminum panel. The stiffness, spacing, and installation accuracy of the keel directly determine whether the aluminum panel can be laid flat, and it is also the most easily simplified and miscalculated link.
1.The spacing between keel arrangements must be calculated mechanically and cannot be determined based on experience
The spacing between keels cannot be simply fixed at a single value. It is necessary to conduct deflection calculations based on the size of the plate, thickness of the aluminum plate, local wind pressure, and building height to control the deformation of the keels under load.
·Vertical keel: The spacing should first match the width of the aluminum plate panel, usually 1200mm~1500mm; Coastal and high wind pressure areas should appropriately reduce the spacing and control the deflection of the keel to meet the specified limits.
·Horizontal keel (secondary keel): As a direct support for aluminum plate panels, the spacing should correspond to the position of the aluminum plate reinforcement ribs, ensuring that there are support points below each reinforcement rib to avoid the aluminum plate being suspended in the middle of the span and deformed by wind loads.
Xcommon mistake: In order to save costs, the spacing between the keel is enlarged, the span of the plate is too large, and the aluminum plate is bent back and forth by wind pressure, forming permanent wave deformation.
2.Selection of keel section and stiffness control
The cross-section of the keel should meet the dual requirements of strength and deflection, and aluminum alloy profiles or hot-dip galvanized steel keels that meet the calculation requirements should be preferred; Perform anti-corrosion repairs on the welded parts of the steel keel to prevent corrosion and deformation in the later stage. Priority should be given to bolted connections for keel connections to reduce thermal deformation caused by on-site welding and avoid twisting of the skeleton itself.
3.Hard control indicators for the accuracy of keel installation
·The verticality deviation of a single vertical keel is ≤ 2mm/m, and the height deviation of the entire layer is strictly controlled;
·Horizontal keel levelness ≤ 1mm/m; The spacing error of the keel grid should be controlled within 5mm;
·After the installation of all keels is completed, they must be rechecked using a ruler and a laser leveler. If the height difference of the keel base exceeds the standard, it cannot be directly placed on the board. It is strictly prohibited to use forced pulling of the aluminum plate or hard adjustment of the corner code board surface to level it, which will introduce huge internal stress to the aluminum plate and directly cause bulging and warping due to temperature changes in the later stage.
4.Key points of nodes and connectors
Elastic gaskets are installed between the keel and the aluminum plate corner brackets to avoid rigid hard contact; The layout of fixed points is uniform and the force is balanced. Pre check the civil engineering structural errors of embedded parts and adapters, digest the deviations of the civil engineering base in advance, and do not leave all civil engineering errors to be compensated by aluminum plate panels.
B、Aluminum plate factory processing: The inherent quality of the plate determines the lower limit of flatness
No matter how good the keel is, if the aluminum plate leaves the factory with insufficient stress and stiffness, it will still deform in the later stage. The flatness control of aluminum plates is of utmost importance in the factory processing stage.
1.Base material selection and sheet thickness control
The standard thickness for single-layer aluminum panels on exterior walls is not less than 2.5mm; for large panels and high wind pressure projects, thicker aluminum panels are required and cannot be blindly reduced. Prioritize the use of aluminum plate substrates that have undergone stress relief treatment. The process of aluminum plate rolling, spraying and curing will generate residual stress; If the spraying and baking temperature is uneven and the cooling is too fast, the internal stress of the board will slowly release with temperature cycling after installation, and waves and bumps will gradually appear. This deformation may not even be visible during factory acceptance, but gradually becomes apparent after delivery, making rectification extremely difficult.
2.Strengthening the reinforcement design is the core of preventing deformation of large aluminum plates
Many aluminum plates have bulges, and the root cause is the unreasonable design of the reinforcing ribs:
The section and spacing of reinforcing bars must be calculated according to the size of the plate and wind pressure, and not just a few aluminum bars pasted randomly;
The length of the reinforcing rib is 3-5mm shorter than the net size inside the aluminum plate, and cannot withstand the folded edges at both ends; To avoid temperature expansion, reinforce the ribs to squeeze the aluminum plate and fold it, causing the surface of the plate to bulge;
Reinforcing ribs and aluminum plates are fixed using a combination of structural adhesive and rivets to ensure a firm bond; The reinforcing ribs must form uniform support on the back of the aluminum plate to ensure uniform stiffness of the plate surface.
X typical error: The two ends of the reinforcing rib are pressed against the folded edge of the aluminum plate, causing temperature rise, thermal expansion compression, and outward bulging of the plate surface.
3. Precision control of sheet metal processing
·CNC bending, bending angle error ≤ ± 1 °;
·The diagonal deviation of the plate should be controlled within ± 2mm;
·Factory board flatness control ≤ 2mm/m; Inspect each piece with a 2m ruler before leaving the factory; Poor consistency in the size of the folded edge and large diagonal deviation can cause forced alignment during corner code installation, resulting in forced pulling of the board and plastic deformation.
4.Spraying, packaging, and transportation protection
The fluorocarbon spray curing process should be stable, strictly control the uniformity of furnace temperature, and reduce thermal stress. Finished aluminum plates should be protected by adding isolation pads between the plates and stacked flat. Single point hanging stacking is prohibited to prevent pre deformation during transportation and stacking.
C、Addendum: Factors that are easily overlooked in on-site installation and temperature stress
The fixing screws/pressure blocks should have uniform force and should not be tightened too tightly at a single point. Local compression may directly press the concave surface of the board; The fixed point spacing shall strictly follow the drawing and cannot be increased arbitrarily;
Reasonable expansion joints should be reserved between aluminum plates. The aluminum plate has a large coefficient of linear expansion, and the temperature difference causes a large amount of expansion and contraction. Insufficient gaps can cause mutual compression and bulging of the plate surface;
Prioritize symmetrical construction from the middle reference plate to both sides in typesetting to reduce cumulative errors; After installing a few boards, check the flatness in a timely manner and do not inspect after completing a large area.
D、Problem rectification ideas (available on project site)
·Slight wave deformation: Review the flatness of the keel, adjust the corner code gasket, and release the internal stress of the board;
·The board has permanent bulging and stress deformation: simply adjusting the angle code cannot repair it, only replacing the board;
·Batch occurrence of uneven board surface: Review and deepen keel calculation, reinforcement drawing, aluminum plate substrate stress, spraying process, and rectify from the source.
Conclusion:
The flatness of the aluminum curtain wall is divided into seven parts for design and processing, and three parts for on-site installation. Many projects pursue exterior facade effects, but compress costs at key points such as keel spacing, aluminum plate reinforcement, and substrate stress, resulting in obvious wavy patterns under sunlight and greatly reduced visual appeal. The cost of later rectification is extremely high. Proper mechanical verification of the keel system, strict control of aluminum plate processing stress, and reinforcement structure are necessary to reduce the unevenness of the board surface from the root and ensure the long-term aesthetic stability of the curtain wall.